焊前预处理对钛合金厚板焊接残余应力的影响 |
| 周牧, 王倩, 王延绪, 翟梓融, 何伦华, 李昺, 马英杰, 雷家峰, 杨锐 |
|
Effect of Prewelding Pretreatment on Welding Residual Stress of Titanium Alloy Thick Plate |
| ZHOU Mu, WANG Qian, WANG Yanxu, ZHAI Zirong, HE Lunhua, LI Bing, MA Yingjie, LEI Jiafeng, YANG Rui |
| 图1 不同残余应力检测方法的取样示意图及中子衍射(ND)法样品放置示意图 |
| Fig.1 Sampling diagram of different residual stress detection methods (unit: mm) (a) and schematic of sample placement for ND method (b) (NDN—normal direction, TD—transverse direction, RD—rolling direction, ND—neutron diffraction, DHD—deep-hole drilling, RN—Rostenthal-Norton) |
|