时效温度对SiC/Al-Zn-Mg-Cu复合材料时效析出行为的影响 |
| 张冉, 朱士泽, 刘振宇, 柯于斌, 王东, 肖伯律, 马宗义 |
|
Influence of Aging Temperatures on Precipitation Behaviors of SiC/Al-Zn-Mg-Cu Composites |
| ZHANG Ran, ZHU Shize, LIU Zhenyu, KE Yubin, WANG Dong, XIAO Bolv, MA Zongyi |
| 图5 15%SiC/7085Al复合材料在100和160℃时效不同时间后的工程应力-应变曲线 |
| Fig.5 Engineering stress-strain curves of 15%SiC/7085Al composites after aging at 100oC (a) and 160oC (b) for different time |
|