深冷循环对SiC/Al复合材料宏微观残余应力的影响 |
| 谷黎明, 冯效铭, 于朝, 张峻凡, 刘振宇, 何伦华, 卢怀乐, 李小虎, 王晨, 张晓东, 肖伯律, 马宗义 |
|
Impact of Cryogenic Cycling on the Macro and Microscopic Residual Stress in SiC/Al Composites |
| GU Liming, FENG Xiaoming, YU Zhao, ZHANG Junfan, LIU Zhenyu, HE Lunhua, LU Huaile, LI Xiaohu, WANG Chen, ZHANG Xiaodong, XIAO Bolv, MA Zongyi |
| 图7 D120试样不同深冷循环后Al相等效塑性应变的分布情况及基体等效塑性应变对比图 |
| Fig.7 Distributions of equivalent plastic strains (PEEQ) in Al phase after different cryogenic cycles of D120 sample (a-g) annealed state (a) and 1-6 cryogenic cyc, respectively (b-g) (h) comparison of equivalent plastic strains in matrix with different number of cryogenic cycles |
|