中子衍射应力分析技术及其应用进展 |
| 林皓, 李建, 杨钊龙, 钟圣怡 |
|
Recent Progress in Stress Analysis Technology and Application of Neutron Diffraction |
| LIN Hao, LI Jian, YANG Zhaolong, ZHONG Shengyi |
| 图8 铁轨残余应力分布中子衍射测试设备及主应力分布示意图[ |
| Fig.8 Neutron diffraction measurement of residual stress distribution on railway tracks (a) and illustration of nominal stress distribution (unit: mm) (b)[ |
|