中子衍射应力分析技术及其应用进展 |
| 林皓, 李建, 杨钊龙, 钟圣怡 |
|
Recent Progress in Stress Analysis Technology and Application of Neutron Diffraction |
| LIN Hao, LI Jian, YANG Zhaolong, ZHONG Shengyi |
| 图7 原位中子衍射实验装置及中子衍射图案[ |
| Fig.7 The setup of in-situ neutron diffraction experiment (a) and a diffraction pattern of CNT/Al sample obtained from neutron diffraction at 2θ = 89° prior to loading (b)[ |
|