贝氏体轨道钢连铸凝固过程中溶质微观偏析模型及分析 |
| 高新亮, 巴文月, 张正, 席仕平, 徐东, 杨志南, 张福成 |
|
Model and Analysis of Solute Microsegregation in Bainite Rail Steel During Continuous Casting Process |
| GAO Xinliang, BA Wenyue, ZHANG Zheng, XI Shiping, XU Dong, YANG Zhinan, ZHANG Fucheng |
| 图9 溶质元素含量和冷却速率对凝固特征温度的影响 |
| Fig.9 Effects of C content (a), Mn content (b), S content (c), P content (d), and cooling rate (e) on solidification characteristic temperatures |
|