贝氏体轨道钢连铸凝固过程中溶质微观偏析模型及分析 |
| 高新亮, 巴文月, 张正, 席仕平, 徐东, 杨志南, 张福成 |
|
Model and Analysis of Solute Microsegregation in Bainite Rail Steel During Continuous Casting Process |
| GAO Xinliang, BA Wenyue, ZHANG Zheng, XI Shiping, XU Dong, YANG Zhinan, ZHANG Fucheng |
| 图4 不同固相率下C含量对溶质元素微观偏析度的影响 |
| Fig.4 Effects of C content on the microsegregation degree of C and Si (a), Mn and Cr (b), Ni and Mo (c), P and S (d) at different fS |
|