构型化石墨烯纳米片/2009Al复合材料热膨胀系数模拟 |
| 周丽, 张明远, 杨欣盛, 刘振宇, 王全兆, 肖伯律, 马宗义 |
|
Simulation of Thermal Expansion Coefficient of Configurational GNPs/2009Al Composites |
| ZHOU Li, ZHANG Mingyuan, YANG Xinsheng, LIU Zhenyu, WANG Quanzhao, XIAO Bolv, MA Zongyi |
| 图19 GNPs/2009Al复合材料热膨胀系数随GNPs体积分数的变化 |
| Fig.19 Thermal expansion coefficients of GNPs/2009Al composites as a function of volume fraction of GNPs |
|