构型化石墨烯纳米片/2009Al复合材料热膨胀系数模拟 |
| 周丽, 张明远, 杨欣盛, 刘振宇, 王全兆, 肖伯律, 马宗义 |
|
Simulation of Thermal Expansion Coefficient of Configurational GNPs/2009Al Composites |
| ZHOU Li, ZHANG Mingyuan, YANG Xinsheng, LIU Zhenyu, WANG Quanzhao, XIAO Bolv, MA Zongyi |
| 图11 典型GNPs几何构型复合材料的RVE模型 |
| Fig.11 Schematics of RVE model with five GNPs configurations (a) layered (b) evenly oriented (c) bundled (d) networked (e) randomly arranged |
|