构型化石墨烯纳米片/2009Al复合材料热膨胀系数模拟 |
| 周丽, 张明远, 杨欣盛, 刘振宇, 王全兆, 肖伯律, 马宗义 |
|
Simulation of Thermal Expansion Coefficient of Configurational GNPs/2009Al Composites |
| ZHOU Li, ZHANG Mingyuan, YANG Xinsheng, LIU Zhenyu, WANG Quanzhao, XIAO Bolv, MA Zongyi |
| 图6 不同GNPs分布形式下GNPs/2009Al复合材料X方向的应力(σ11)分布 |
| Fig.6 X-direction stress (σ11) distributions of GNPs/2009Al composites with different GNPs distributions (a) one cluster (b) two clusters (c) four clusters (d) eight clusters |
|