构型化石墨烯纳米片/2009Al复合材料热膨胀系数模拟 |
| 周丽, 张明远, 杨欣盛, 刘振宇, 王全兆, 肖伯律, 马宗义 |
|
Simulation of Thermal Expansion Coefficient of Configurational GNPs/2009Al Composites |
| ZHOU Li, ZHANG Mingyuan, YANG Xinsheng, LIU Zhenyu, WANG Quanzhao, XIAO Bolv, MA Zongyi |
| 图1 石墨烯纳米片(GNPs)/2009Al复合材料的代表性体积元(RVE)模型 |
| Fig.1 Representative volume element (RVE) model of graphene nanoplatelets (GNPs)/2009Al composites (a) whole model (b) meshing (Inset shows the local mesh refinement) |
|