Nb3Sn超导线材中Ta层的去除及腐蚀机理 |
| 高瞻, 张泽荣, 程军胜, 王秋良 |
|
Removal of Tantalum Layer from Nb3Sn Superconducting Wire and Corrosion Mechanism |
| GAO Zhan, ZHANG Zerong, CHENG Junsheng, WANG Qiuliang |
| 图10 Ta片腐蚀前后的XRD谱 |
| Fig.10 XRD spectra of uncorroded and corroded tantalum sheets |
|