Nb3Sn超导线材中Ta层的去除及腐蚀机理 |
| 高瞻, 张泽荣, 程军胜, 王秋良 |
|
Removal of Tantalum Layer from Nb3Sn Superconducting Wire and Corrosion Mechanism |
| GAO Zhan, ZHANG Zerong, CHENG Junsheng, WANG Qiuliang |
| 图4 Nb3Sn超导线材在酸溶液中的腐蚀方式 |
| Fig.4 Corrosion modes of Nb3Sn superconducting wire in the acid solutions |
|