Nb3Sn超导线材中Ta层的去除及腐蚀机理 |
| 高瞻, 张泽荣, 程军胜, 王秋良 |
|
Removal of Tantalum Layer from Nb3Sn Superconducting Wire and Corrosion Mechanism |
| GAO Zhan, ZHANG Zerong, CHENG Junsheng, WANG Qiuliang |
| 图2 Nb3Sn超导线分层结构横截面的OM像 |
| Fig.2 Cross-sectional OM image of Nb3Sn superconducting wire layered structure |
|