(111)取向纳米孪晶Cu的抗氧化性能及焊料润湿性 |
| 许增光, 周士祺, 李晓, 刘志权 |
|
Excellent Oxidation Resistance and Solder Wettability of (111)-Oriented Nanotwinned Cu |
| XU Zengguang, ZHOU Shiqi, LI Xiao, LIU Zhiquan |
| 图9 (111)nt-Cu和C-Cu样品氧化前表面的晶粒取向差角分布和晶粒尺寸分布 |
| Fig.9 Grain misorientation distributions (a, b) and grain size distributions (c, d) of (111)nt-Cu (a, c) and C-Cu (b, d) samples |
|