| 图10 Co-20Ni-8Cr-xAl四元合金与Co-20Ni-xAl三元合金[ |
| Fig.10 Comparisons of the kinetic curves for the oxi-dation in 1.013 × 105 Pa O2 at 800oC (a), 900oC (b), and 1000oC (c) for 20 h of the quaternary Co-20Ni-8Cr-xAl alloys with the corresponding data for the ternary Co-20Ni-xAl[ |
|