四元Co-Ni-Cr-Al合金高温氧化模式及其转变机理 |
| 吕云蕾, 任延杰, 冯抗抗, 周梦妮, 王文, 陈荐, 牛焱 |
|
High Temperature Oxidation Mode and Transformation Mechanism of Quaternary Co-Ni-Cr-Al Alloys |
| LV Yunlei, REN Yanjie, FENG Kangkang, ZHOU Mengni, WANG Wen, CHEN Jian, NIU Yan |
| 图2 Co-20Ni-8Cr-3Al和Co-20Ni-8Cr-5Al合金在800、900、1000和1100℃下1.013 × 105 Pa O2中氧化20 h的动力学曲线 |
| Fig.2 Kinetic curves for oxidation of the Co-20Ni-8Cr-3Al (a) and Co-20Ni-8Cr-5Al (b) alloys in 1.013 × 105 Pa O2 at 800, 900, 1000, and 1100oC for 20 h |
|