共晶组织强化NbMoZrVSi x 难熔高熵合金的摩擦磨损性能及磨损机理 |
| 王瀚铭, 杜银, 裴旭辉, 王海丰 |
|
Tribological Property and Wear Mechanism of NbMoZrVSi x Refractory High-Entropy Alloy Strengthened by Eutectic Structure |
| WANG Hanming, DU Yin, PEI Xuhui, WANG Haifeng |
| 图5 Si0~Si0.2合金的显微硬度 |
| Fig.5 Hardnesses of Si0-Si0.2 alloys |
|