共晶组织强化NbMoZrVSi x 难熔高熵合金的摩擦磨损性能及磨损机理 |
| 王瀚铭, 杜银, 裴旭辉, 王海丰 |
|
Tribological Property and Wear Mechanism of NbMoZrVSi x Refractory High-Entropy Alloy Strengthened by Eutectic Structure |
| WANG Hanming, DU Yin, PEI Xuhui, WANG Haifeng |
| 图4 Si0.1合金中的共晶组织BSE像及EDS元素分布图 |
| Fig.4 BSE image and EDS element distribution maps of Si0.1 alloy eutectic structure (a) BSE image of Si0.1 alloy (b) high magnification image of eutectic structure in Fig.4a and EDS mappings |
|