铸型正反转搅动对精密铸造K4169合金凝固组织和室温力学性能的影响 |
| 陈诚, 杨光昱, 金梦辉, 王强, 汤鑫, 程会民, 介万奇 |
|
Effect of the Mold Positive and Negative Rotation on the Microstructure and Room-Temperature Mechanical Properties of K4169 Superalloy |
| CHEN Cheng, YANG Guangyu, JIN Menghui, WANG Qiang, TANG Xin, CHENG Huimin, JIE Wanqi |
| 图7 K4169高温合金铸态组织中基体和不同第二相的显微硬度 |
| Fig.7 Microhardness of matrix and different second phases in the as-cast K4169 superalloy |
|