铸型正反转搅动对精密铸造K4169合金凝固组织和室温力学性能的影响 |
| 陈诚, 杨光昱, 金梦辉, 王强, 汤鑫, 程会民, 介万奇 |
|
Effect of the Mold Positive and Negative Rotation on the Microstructure and Room-Temperature Mechanical Properties of K4169 Superalloy |
| CHEN Cheng, YANG Guangyu, JIN Menghui, WANG Qiang, TANG Xin, CHENG Huimin, JIE Wanqi |
| 图6 K4169高温合金组织中各相及其EDS分析位置 |
| Fig.6 Phases and its EDS analysis locations in the K4169 superalloy (a) bulk Laves phase (b) eutectic Laves phase (c) MC phase |
|