1Cr22Mn16N高氮奥氏体不锈钢塑性变形连接中界面组织演化及愈合机制 |
| 杨瑞泽, 翟汝宗, 任少飞, 孙明月, 徐斌, 乔岩欣, 杨兰兰 |
|
Evolution and Healing Mechanism of 1Cr22Mn16N High Nitrogen Austenitic Stainless Steel Interface Microstructure During Plastic Deformation Bonding |
| YANG Ruize, ZHAI Ruzong, REN Shaofei, SUN Mingyue, XU Bin, QIAO Yanxin, YANG Lanlan |
| 图4 1200℃时不同变形量的1Cr22Mn16N HNASS界面处的OM像和平均晶粒尺寸图 |
| Fig.4 OM images of interface in 1Cr22Mn16N HNASS at 1200oC and deformations of 10% (a), 20% (b), 30% (c), and 40% (d); and average grain size diagram (e) |
|