1Cr22Mn16N高氮奥氏体不锈钢塑性变形连接中界面组织演化及愈合机制 |
| 杨瑞泽, 翟汝宗, 任少飞, 孙明月, 徐斌, 乔岩欣, 杨兰兰 |
|
Evolution and Healing Mechanism of 1Cr22Mn16N High Nitrogen Austenitic Stainless Steel Interface Microstructure During Plastic Deformation Bonding |
| YANG Ruize, ZHAI Ruzong, REN Shaofei, SUN Mingyue, XU Bin, QIAO Yanxin, YANG Lanlan |
| 图1 实验方法及样品尺寸示意图 |
| Fig.1 Schematics of the experimental method and sample size (unit: mm) (a) experimental method of plastic deformation bonding (b) samples before and after deformation (c) experimental method of tensile butt-joint (The top schematic shows a butt-joint specimen; the bottom schematic shows the sample of the base material) (d) tensile sample before compression |
|