Ga添加对304L不锈钢力学性能和抗菌性能的影响 |
| 孟玉佳, 席通, 杨春光, 赵金龙, 张新蕊, 于英杰, 杨柯 |
|
Effect of Gallium Addition on Mechanical and Antibacterial Properties of 304L Stainless Steel |
| MENG Yujia, XI Tong, YANG Chunguang, ZHAO Jinlong, ZHANG Xinrui, YU Yingjie, YANG Ke |
| 图8 304L-Ga不锈钢在37℃与不同溶液共培养24 h后析出的Ga3+浓度 |
| Fig.8 Ga3+ concentrations in different solutions after co-cultured with 304L-Ga SS at 37oC for 24 h (PBS—phosphate buffer solution) |
|