Ga添加对304L不锈钢力学性能和抗菌性能的影响 |
| 孟玉佳, 席通, 杨春光, 赵金龙, 张新蕊, 于英杰, 杨柯 |
|
Effect of Gallium Addition on Mechanical and Antibacterial Properties of 304L Stainless Steel |
| MENG Yujia, XI Tong, YANG Chunguang, ZHAO Jinlong, ZHANG Xinrui, YU Yingjie, YANG Ke |
| 图5 E. coli和S. mutans与304L和304L-Ga不锈钢共培养后生长的菌落情况及304L-Ga不锈钢的抗菌率 |
| Fig.5 Bacterial colonies of E. coli and S. mutans after co-culture with 304L SS and 304L-Ga SS (a) and the antibacterial rates of 304L-Ga SS against E. coli and S. mutans (b) |
|