预变形对双峰分离非基面织构AZ31镁合金板材室温力学行为及微观组织演变的影响 |
| 汪丽佳, 胡励, 苗天虎, 周涛, 何曲波, 刘相果 |
|
Effect of Pre-Deformation on Mechanical Behavior and Microstructure Evolution of AZ31 Mg Alloy Sheet with Bimodal Non-Basal Texture at Room Temperature |
| WANG Lijia, HU Li, MIAO Tianhu, ZHOU Tao, HE Qubo, LIU Xiangguo |
| 图4 RD试样单轴拉伸3%和6%条件下的EBSD分析 |
| Fig.4 EBSD analyses of RD samples deformed to the deformation 3% (a-c) and 6% (d-f) (HAGB—high angle grain boundary, LAGB—low angle grain boundary) (a, d) IPFs (b, e) grain boundary (GB) maps (c, f) kernel average misorientation (KAM) maps |
|