预变形对双峰分离非基面织构AZ31镁合金板材室温力学行为及微观组织演变的影响 |
| 汪丽佳, 胡励, 苗天虎, 周涛, 何曲波, 刘相果 |
|
Effect of Pre-Deformation on Mechanical Behavior and Microstructure Evolution of AZ31 Mg Alloy Sheet with Bimodal Non-Basal Texture at Room Temperature |
| WANG Lijia, HU Li, MIAO Tianhu, ZHOU Tao, HE Qubo, LIU Xiangguo |
| 图1 实验流程及拉伸试样取样方式和相应尺寸示意图 |
| Fig.1 Schematics of experiment procedure (a), and the sampling method and the corresponding dimension of manufactured tensile sample (b) (TD—transverse direction, RD—rolling direction. unit: mm) |
|