TC19合金铸锭中Zr、Mo元素的宏观偏析行为
朱绍祥, 王清江, 刘建荣, 陈志勇

Macrosegregation of Zr and Mo in TC19 Titanium Alloy Ingot
ZHU Shaoxiang, WANG Qingjiang, LIU Jianrong, CHEN Zhiyong
图6 利用JMatPro软件计算TC19合金固液相变时密度变化
Fig.6 Densities of TC19 alloy calculated by JMatPro software at 1630-1730oC