AlSi10Mg多孔结构在不同加载应变率下的损伤模式及响应机制 |
| 蔡宣明, 张伟, 范志强, 高玉波, 王俊元, 张柱军 |
|
Damage Modes and Response Mechanisms of AlSi10Mg Porous Structures Under Different Loading Strain Rates |
| CAI Xuanming, ZHANG Wei, FAN Zhiqiang, GAO Yubo, WANG Junyuan, ZHANG Zhujun |
| 图8 高速相机拍摄到的AlSi10Mg多孔结构在1137 s-1高应变率加载条件下的变形及破坏模式 |
| Fig.8 Deformation and failure modes of AlSi10Mg porous structure under high strain rate loading of 1137 s-1 captured by high-speed camera for 0 μs (a), 50 μs (b), 100 μs (c), 150 μs (d), and 200 μs (e) (v—impact velocity of the striker) |
|