AlSi10Mg多孔结构在不同加载应变率下的损伤模式及响应机制 |
| 蔡宣明, 张伟, 范志强, 高玉波, 王俊元, 张柱军 |
|
Damage Modes and Response Mechanisms of AlSi10Mg Porous Structures Under Different Loading Strain Rates |
| CAI Xuanming, ZHANG Wei, FAN Zhiqiang, GAO Yubo, WANG Junyuan, ZHANG Zhujun |
| 图6 AlSi10Mg多孔结构在低应变率(0.009 s-1)下的变形破坏模式及破坏位置示意图 |
| Fig.6 Deformation failure mode (a-d, f-i, k-n) and schematics of damage location (dash lines) (e, j, o) at the first region (a-e), the second region (f-j), and the third region (k-o) of AlSi10Mg porous structure at low strain rates (0.009 s-1) (elastic deformation, the strain ε ≈ 2%; first fracture, ε ≈ 6.7%; collapse, ε ≈ 30%) |
|