AlSi10Mg多孔结构在不同加载应变率下的损伤模式及响应机制 |
| 蔡宣明, 张伟, 范志强, 高玉波, 王俊元, 张柱军 |
|
Damage Modes and Response Mechanisms of AlSi10Mg Porous Structures Under Different Loading Strain Rates |
| CAI Xuanming, ZHANG Wei, FAN Zhiqiang, GAO Yubo, WANG Junyuan, ZHANG Zhujun |
| 图1 AlSi10Mg多孔结构优化及设计的主要成形模式示意图 |
| Fig.1 Schematics of main forming modes for optimization and design of AlSi10Mg porous structure (δ—wall thickness) |
|