Y掺杂Ti膜的吸放氢行为 |
| 李聪, 王猛, 屠汉俊, 施立群 |
|
Behavior of Hydrogen Absorption and Desorption in Y-doped Ti Films |
| LI Cong, WANG Meng, TU Hanjun, SHI Liqun |
| 图13 TiD0.63和TiY0.13D0.78样品的升温速率与热脱附峰峰温的关系 |
| Fig.13 Relationships between heating rate (v) and thermal desorption peak temperature (TP) of TiD0.63 and TiY0.13D0.78 (R2—goodness of fit) |
|