Y掺杂Ti膜的吸放氢行为 |
| 李聪, 王猛, 屠汉俊, 施立群 |
|
Behavior of Hydrogen Absorption and Desorption in Y-doped Ti Films |
| LI Cong, WANG Meng, TU Hanjun, SHI Liqun |
| 图8 吸氘后不同Y含量的Ti薄膜中的D浓度分布 |
| Fig.8 Depth profiles of D concentration in Ti films with Y concentration after absorbing deuterium (Dashed lines indicate estimated values) |
|