Cu-V双合金化3Mn钢的组织和力学性能 |
| 许仁杰, 屠鑫, 胡斌, 罗海文 |
|
Microstructure and Mechanical Properties of Cu-V Dual Alloyed 3Mn Steel |
| XU Renjie, TU Xin, HU Bin, LUO Haiwen |
| 图4 温轧退火以及热轧时效退火组织的EBSD质量图与相分布叠加图 |
| Fig.4 EBSD band contrast images overlapped with phase distribution on the microstructures of WR-IA and Aging-IA specimens (a) WR550-690 (b) WR600-690 (c) WR650-690 (d) HR550-690 (e) HR600-690 (f) HR650-690 |
|