铁素体系耐热钢焊接热影响区相变行为的CSLM原位观察 |
| 申洋, 谷征满, 王聪 |
|
Phase Transformation Behaviors in the Heat-Affected Zones of Ferritic Heat-Resistant Steels Enabled by In Situ CSLM Observation |
| SHEN Yang, GU Zhengman, WANG Cong |
| 图7 P91铁素体耐热钢FGHAZ冷却过程中马氏体板条长大过程的CSLM像 |
| Fig.7 CSLM images of the growth of martensite laths in the FGHAZ of P91 ferritic heat-resistant steel (a-f) |
|