铁素体系耐热钢焊接热影响区相变行为的CSLM原位观察 |
| 申洋, 谷征满, 王聪 |
|
Phase Transformation Behaviors in the Heat-Affected Zones of Ferritic Heat-Resistant Steels Enabled by In Situ CSLM Observation |
| SHEN Yang, GU Zhengman, WANG Cong |
| 图4 P22铁素体耐热钢CGHAZ冷却过程中贝氏体板条长大过程的CSLM像 |
| Fig.4 CSLM images of the growth of bainite laths in the CGHAZ of P22 ferritic heat-resistant steel (a-i) (Insets show partial enlarged bainite laths) |
|