Ni含量对高强度低合金钢淬透性影响的晶体学认识 |
| 苏帅, 韩鹏, 杨善武, 王华, 金耀辉, 尚成嘉 |
|
Crystallographic Understanding of the Effect of Ni Content on the Hardenability of High-Strength Low-Alloy Steel |
| SU Shuai, HAN Peng, YANG Shanwu, WANG Hua, JIN Yaohui, SHANG Chengjia |
| 图2 0.92Ni钢和2.94Ni钢的连续冷却转变(CCT)曲线 |
| Fig.2 Continuous cooling transition (CCT) curves of 0.92Ni steel and 2.94Ni steel (Ms—starting temperature of martensitic transformation, Ts—starting temperature of phase transformation at each cooling rate, Tf—finishing temperature of phase transformation at each cooling rate) |
|