局部强冷作用下厚板铝合金/镁合金搅拌摩擦焊界面金属间化合物的析出行为 |
| 徐洋, 柯黎明, 聂浩, 夏春, 刘强, 陈书锦 |
|
Precipitation Behavior of Intermetallic Compounds at the Interface of Thick Plate Friction Stir Welded Al Alloy/Mg Alloy Joints Under Local Strong Cooling |
| XU Yang, KE Liming, NIE Hao, XIA Chun, LIU Qiang, CHEN Shujin |
| 图11 表面液氮冷却时5A06-H112/AZ31B-O FSW接头镁合金侧界面底部IMCs层的HADDF像、元素分布和SAED花样 |
| Fig.11 HADDF image (a), element distributions (b, c), and SAED patterns (d, e) of IMCs layer at the bottom of Mg alloy side interface of 5A06-H112/AZ31B-O FSW joint under liquid nitrogen cooling |
|