| 局部强冷作用下厚板铝合金/镁合金搅拌摩擦焊界面金属间化合物的析出行为 | 
| 徐洋, 柯黎明, 聂浩, 夏春, 刘强, 陈书锦 | 
| Precipitation Behavior of Intermetallic Compounds at the Interface of Thick Plate Friction Stir Welded Al Alloy/Mg Alloy Joints Under Local Strong Cooling | 
| XU Yang, KE Liming, NIE Hao, XIA Chun, LIU Qiang, CHEN Shujin | 
| 图4 空冷和表面液氮冷却时5A06-H112/AZ31B-O FSW接头的宏观形貌 | 
| Fig.4 Surface (a, c) and cross-sectional (b, d) morphologies of 5A06-H112/AZ31B-O FSW joints under air (a, b) and liquid nitrogen (c, d) cooling (SZ—stir zone, Wlower—width of lower stir zone) | 
|   |