不锈钢纤维增强镁基仿生复合材料制备与力学性能 |
| 谢丽文, 张立龙, 刘艳艳, 张明阳, 王绍钢, 焦大, 刘增乾, 张哲峰 |
|
Fabrication and Mechanical Properties of Bioinspired Mg-Based Composites Reinforced by Stainless Steel Fibers |
| XIE Liwen, ZHANG Lilong, LIU Yanyan, ZHANG Mingyang, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng |
| 图3 具有不同微观结构的不锈钢纤维增强镁基复合材料沿厚度方向截面二维微观形貌的SEM像 |
| Fig.3 SEM images of the through-thickness cross-sections of the Mg-based composites with random stacking (a), orthogonal plywood (b), and double-Bouligand (c) architectures (Light gray: stainless steel fiber; dark gray: Mg matrix) |
|