Alloy mass fraction / % | Alloy with peak HTS mass fraction / % | Alloy with valley HTS mass fraction / % | Processing parameter |
---|
Tmold / oC | Tpour / oC |
---|
Mg-1.5Zn-xY (x = 0.2, 2, 4)[37] | Mg-1.5Zn-0.2Y | Mg-1.5Zn-4Y | 250 | 750 | Mg-4.5Zn-xY (x = 0, 0.4, 0.9, 2)[38] | Mg-4.5Zn-0.4Y Mg-4.5Zn-0.9Y | Mg-4.5Zn-2Y | 250 | 750 | Mg-4.5Zn-0.9Y | Mg-4.5Zn, Mg-4.5Zn-2Y | 450 | 750 | Mg-xZn-2xY (x = 1, 1.67, 2.67)[39] | Mg-1.67Zn-3.34Y | Mg-2.67Zn-5.34Y | 250 | 720 | Mg-4.5Zn-xY-0.5Zr (x = 0.5, 1, 2, 4, 6)[40] | Mg-4.5Zn-1Y-0.5Zr | Mg-4.5Zn-6Y-0.5Zr | 200 | 720 | Mg-1Zn-xY (x = 1, 1.33, 2)[41] | Mg-1Zn-1Y | Mg-1Zn-1.33Y | 250 | 750 | Mg-1Zn-xY (x = 1, 2, 3)[42] | Mg-1Zn-1Y | Mg-1Zn-3Y | 250 | 750 | Mg-6.5Zn-xY-0.5Zr (x = 1, 2, 4, 6)[43] | Mg-6.5Zn-6Y-0.5Zr | Mg-6.5Zn-2Y-0.5Zr | 200 | 720 | Mg-5(Zn + Y)-0.5Zr (Mg-2.5Zn-2.5Y-0.5Zr, Mg-3Zn-2Y-0.5Zr, Mg-3.75Zn-1.25Y-0.5Zr, Mg-4.29Zn-0.71Y-0.5Zr)[44] | Mg-3.75Zn-1.25Y-0.5Zr | Mg-2.5Zn-2.5Y-0.5Zr | 200 | 700 | Mg-xZn-0.5Y-0.5Zr (x = 1.5, 2.5, 3.5, 4.5)[45] | Mg-1.5Zn-0.5Y-0.5Zr | Mg-4.5Zn-0.5Y-0.5Zr | 280 | 700 | Mg-xZn-2Y (x = 0, 0.5, 1.5, 4.5)[46] | Mg-1.5Zn-2Y | Mg-2Y | 250 | 750 | Mg-xZn-4Y-0.5Zr (x = 0, 0.5, 1.5, 3)[47] | Mg-1.5Zn-4Y-0.5Zr | Mg-4Y-0.5Zr | 200 | 720 |
|