Mg-Zn系合金热裂行为的研究进展 |
| 王峰, 白盛巍, 王志, 杜旭东, 周乐, 毛萍莉, 魏子淇, 李瑾伟 |
|
Research Progress on Hot Tearing Behavior of Mg-Zn Series Alloys |
| WANG Feng, BAI Shengwei, WANG Zhi, DU Xudong, ZHOU Le, MAO Pingli, WEI Ziqi, LI Jinwei |
| 图4 低频交变磁场处理下MgZnCu相团聚和球化示意图,及MgZnCu相的SEM像[ |
| Fig.4 Schematics of the MgZnCu phase agglomeration and spheroidization under LAMF (a-d, f) and SEM images of MgZnCu phase (e, g, h)[ |
|