Mg-Zn系合金热裂行为的研究进展 |
| 王峰, 白盛巍, 王志, 杜旭东, 周乐, 毛萍莉, 魏子淇, 李瑾伟 |
|
Research Progress on Hot Tearing Behavior of Mg-Zn Series Alloys |
| WANG Feng, BAI Shengwei, WANG Zhi, DU Xudong, ZHOU Le, MAO Pingli, WEI Ziqi, LI Jinwei |
| 图2 外加交变磁场的“T”型热裂测试装置示意图[ |
| Fig.2 Schematic of “T”-shaped hot tearing test system with magnetic field[ |
|