Ni-Cr合金在富CO2 气氛中的高温腐蚀研究进展 |
| 谢云, Zhang Jianqiang, 彭晓 |
|
Research Advances in High Temperature Corrosion of Ni-Cr Alloys in CO2-Rich Environments |
| XIE Yun, Zhang Jianqiang, PENG Xiao |
| 图7 Ni-30Cr-2Ti合金在700℃下Ar + 20CO2 + 20H2O气氛中腐蚀不同时间后的碳化物SEM像[ |
| Fig.7 SEM images of carbide precipitates in Ni-30Cr-2Ti alloy exposed at 700oC for 20 h (a) and 500 h (b) in Ar + 20CO2 + 20H2O[ |
|