Ni-Cr合金在富CO2 气氛中的高温腐蚀研究进展 |
| 谢云, Zhang Jianqiang, 彭晓 |
|
Research Advances in High Temperature Corrosion of Ni-Cr Alloys in CO2-Rich Environments |
| XIE Yun, Zhang Jianqiang, PENG Xiao |
| 图6 Ni-25Cr合金在不同温度下Ar + 20CO2气氛中腐蚀500 h后的截面SEM像[ |
| Fig.6 Cross-sectional SEM images of Ni-25Cr alloy exposed at 650oC (a), 700oC (b), and 800oC (c) for 500 h in Ar + 20CO2[ |
|