Ni-Cr合金在富CO2 气氛中的高温腐蚀研究进展 |
| 谢云, Zhang Jianqiang, 彭晓 |
|
Research Advances in High Temperature Corrosion of Ni-Cr Alloys in CO2-Rich Environments |
| XIE Yun, Zhang Jianqiang, PENG Xiao |
| 图5 Ni-30Cr合金在800℃下Ar + 20CO2 + 20H2O和Ar + 20CO2气氛中腐蚀500 h后的截面SEM像和TEM像[ |
| Fig.5 Cross-sectional SEM images of Ni-30Cr alloy exposed at 800oC for 500 h in Ar + 20CO2 + 20H2O (a) and Ar + 20CO2 (b), and cross-sectional BF-TEM images of corresponding scales formed in Ar + 20CO2 + 20H2O (c, d) and Ar + 20CO2 (e) (Fig.5c is the magnified image at the scale-alloy interface formed in Ar + 20CO2 + 20H2O)[ |
|