Ni-Cr合金在富CO2 气氛中的高温腐蚀研究进展 |
| 谢云, Zhang Jianqiang, 彭晓 |
|
Research Advances in High Temperature Corrosion of Ni-Cr Alloys in CO2-Rich Environments |
| XIE Yun, Zhang Jianqiang, PENG Xiao |
| 图4 Ni-15Cr合金和纯Ni在650℃下Ar + 20CO2和Ar + 20CO2 + 20H2O气氛中腐蚀后的截面SEM像[ |