Ni-Cr合金在富CO2 气氛中的高温腐蚀研究进展 |
| 谢云, Zhang Jianqiang, 彭晓 |
|
Research Advances in High Temperature Corrosion of Ni-Cr Alloys in CO2-Rich Environments |
| XIE Yun, Zhang Jianqiang, PENG Xiao |
| 图2 Ni-25Cr和Ni-30Cr合金在700℃下Ar + 20CO2气氛中腐蚀500 h后晶界碳化物的SEM像[ |
| Fig.2 SEM images of carbides precipitated along the grain boundaries in Ni-25Cr (a) and Ni-30Cr (b) exposed at 700oC for 500 h in Ar + 20CO2 atmosphere[ |
|