高Cr马氏体耐热钢的协同强化机制及形变热处理应用 |
| 张竟文, 余黎明, 刘晨曦, 丁然, 刘永长 |
|
Synergistic Strengthening of High-Cr Martensitic Heat-Resistant Steel and Application of Thermo-Mechanical Treatments |
| ZHANG Jingwen, YU Liming, LIU Chenxi, DING Ran, LIU Yongchang |
| 图11 高Cr马氏体耐热钢焊接过程中FGHAZ中元素偏聚引发的M23C6相不均匀分布及蠕变裂纹[ |
| Fig.11 Element accumulation (a), uneven distribution of M23C6 (b), and creep cracks (c) in FGHAZ in high-Cr martensitic heat-resistant steels[ |
|