高Cr马氏体耐热钢的协同强化机制及形变热处理应用 |
| 张竟文, 余黎明, 刘晨曦, 丁然, 刘永长 |
|
Synergistic Strengthening of High-Cr Martensitic Heat-Resistant Steel and Application of Thermo-Mechanical Treatments |
| ZHANG Jingwen, YU Liming, LIU Chenxi, DING Ran, LIU Yongchang |
| 图6 高温蠕变过程中初始态及20%冷轧态G115钢中富Cu相与位错之间的交互作用,及45%冷轧态G115钢中的位错胞结构及蠕变过程中沉淀相的快速粗化[ |
| Fig.6 Interactions between Cu-rich particles and dislocations in the G115 steel for initial state (a) and 20% cold rolling (c); and dislocation cells for initial state (b) and coarse precipitates after creep rupture (d) in the G115 steel with 45% cold rolling[ |
|